The different material from LDPE and HDPE
Dec 27, 2024
Differences and Comparisons between HDPE and LDPE Materials
Production Methods
- HDPE: It is produced by the low-pressure method, including liquid-phase methods (such as solution and slurry processes) and gas-phase methods.
- LDPE: It is obtained by free radical polymerization of polymerization-grade ethylene with oxygen or peroxide as an initiator under high temperature and high pressure, also known as high-pressure polyethylene.

Structure and Properties
- Density: The density of HDPE is 0.941 - 0.965 g/cm³, while that of LDPE is 0.910 - 0.940 g/cm³.
- Hardness and Rigidity: HDPE has high hardness and rigidity due to its long molecular chains and high crystallinity; LDPE is soft and flexible with short molecular chains and low crystallinity.
- Chemical Resistance: HDPE has good chemical resistance and can resist the erosion of many solvents and chemicals; LDPE has relatively poor chemical resistance.
- Melting Temperature: The melting temperature of HDPE is between 126 - 135 °C, and that of LDPE is usually 105 - 115 °C.
- Mechanical Strength: HDPE has good mechanical strength, such as high tensile, bending, compressive, and shear strength; LDPE has relatively poor mechanical strength.
- Moisture and Waterproof Performance: HDPE has low permeability to water, water vapor, and air, with low water absorption, good moisture and gas barrier properties; LDPE has relatively poor moisture and gas barrier properties.
Appearance
- HDPE: In its original state, it is milky white and appears translucent to a certain extent in a thin cross-section, with relatively low transparency.
- LDPE: It is in the form of milky white spherical particles, with a dull surface and a certain degree of transparency.
Processing Performance
- HDPE: It requires a relatively high processing temperature, usually around 180 °C, and is suitable for various processing methods such as extrusion, blow molding, injection molding, and rotational molding.
- LDPE: It has a lower processing temperature, about 160 °C, and has good formability, applicable to injection molding, extrusion, blow molding, rotational molding, and other processes.